Aluminium · TIG

Aluminium welding to drawing

TIG welding of aluminium profiles, sheets and assemblies in our workshop in Požarevac, Serbia. Before quoting we check the alloy, thickness, joint type and appearance requirements.

Material specifics

Why aluminium is more demanding than steel

Aluminium is covered by an oxide layer that melts at a far higher temperature than the metal itself. If it is not removed, it hinders fusion and causes weld defects.

Aluminium conducts heat quickly and expands more when heated, so distortion is greater than with steel. Moisture and contamination on the surface or wire lead to porosity, so cleaning immediately before welding is a mandatory step.

AC TIG welding breaks up the oxide layer and allows precise heat control, especially on thinner sheets and visible joints.

TIG welding (141) →

What to include in the enquiry

  • Alloy and temper, e.g. EN AW-6082 T6 or EN AW-5754 H111.
  • Sheet or wall thicknesses and the joint type.
  • Appearance requirements and critical dimensions that must not change.
  • Quantity, lead time and whether you supply the material.

We do not currently publish photographs of aluminium work from other jobs; examples can be provided with an enquiry where possible.

Technical requirements

What determines aluminium joint quality

We check these points before quoting, as they affect both price and lead time.

Oxide layer

Removed mechanically just before welding and broken up by alternating current during TIG welding.

Cleanliness

Degreasing and dry filler wire reduce the risk of porosity.

Filler metal

Wire (e.g. AlSi5 or AlMg5) is chosen according to the base alloy and the joint’s purpose.

Distortion

Tacking, fixtures and welding sequence limit bending of profiles and sheets.

Strength in the HAZ

In heat-treated alloys strength drops in the heat-affected zone; this is considered in the design.

Quality level

State the required imperfection level for aluminium (EN ISO 10042) on the drawing, if defined.

FAQ

Aluminium welding — questions before a quotation

Send a drawing, or a photograph of the part with dimensions and the alloy designation.

Send a technical enquiry →
Which aluminium alloys do you weld?

Mostly weldable 5000 and 6000 series alloys, e.g. EN AW-5754, 6060 and 6082. State the exact designation and temper (e.g. T6) and we will confirm feasibility and the filler metal.

Do you repair aluminium parts?

Repairs are assessed individually after inspecting the part. For castings and parts of unknown composition the result cannot be guaranteed in advance, so we clarify this before starting.

How much does aluminium distort during welding?

Aluminium conducts heat quickly and expands more than steel, so distortion is more pronounced. We limit it with tacking, fixtures and welding sequence, but critical dimensions should be marked on the drawing.

Is the welded joint as strong as the base metal?

For heat-treated alloys (e.g. 6082-T6) strength in the heat-affected zone decreases. This is a material property the designer needs to take into account.

Related services

The process follows the joint

One assembly often combines several processes and operations. The final scope is confirmed in the written quotation.

TIG welding (141)

Stainless steel, aluminium, copper and thinner walls; pipes and flanges where appearance and root control matter.

TIG welding →

Stainless steel welding

Root shielding, heat tint, segregated tools and a finish that suits the application.

Stainless steel welding →

MIG/MAG welding

Carbon steel, brackets, frames and longer seams where productive fabrication matters.

MIG/MAG welding →

Next step

Send the drawing of your aluminium item.

State the alloy, thicknesses, quantity, appearance requirements and lead time.